Welcome to our new Instron Community Blog hosted by Instron. It is a compilation of the freshest, brightest, most-talented minds that Instron has to offer. The world of materials science is so vast and encompasses the broadest range of industries, materials, and challenges that no one person can possibly possess all the knowledge required to be the resident expert – or master of materials science. It takes a small army behind the scenes collaborating and sharing technical know-how, experiences, and ideas to present the most accurate, relevant, and timely information to you – our readers.

We invite you to tell us who you are, share your stories and talk about your experiences. Join the Instron Community.

Friday, June 7, 2013

What is Stress Whitening, and How Can It Impact Your Test?


Thermoplastic polymers may exhibit a change in color under tension.  This phenomenon is known as stress whitening and may occur in both semi-crystalline and amorphous thermoplastics.

What is really happening here?

When an axial load is applied to a thermoplastic, the polymer chains reorganize during stretch.  The polymer chains will straighten, slip and shear within the plastic’s microenvironment.  In some cases, occlusions or holes are formed by the movement of fillers and the polymer chains.  Together these occlusions form microvoids.  When microvoids cluster to a size greater than or equal to the wavelength of light (380-750nm), the transmitted light is scattered and the object appears white.  Thus, the microvoids change the refractive index of the plastic.

It is important to understand stress whitening when measuring strain after yield with a video extensometer.  When testing with a video extensometer, contrasting dots are used to track specimen strain (i.e. white dots on a black specimen).  In a stress whitening plastic, a dark specimen marked with white dots will change color after yield.  In this scenario, the video may have difficulty tracking the dots and a more complicated marking solution would be needed.  An alternative solution for measuring strain after yield in stress whitening plastics is to use a high travel contacting extensometer, such as the AutoX750.